This is a really old chunk of Cebloplast...1920-30's. It was what the finest Italian pens were made at that time. It does not tolerate heat in any way, shape or form. 30 minutes to drill and then more to find a better way to turn it. Thankfully it worked!! Blue Ice cobloplast on a chrome Sierra Vista wet sand only to 6k and Huts. Thanks for looking!